摘要
针对张家港浦项不锈钢有限公司带钢表面条状色差问题,对其产生原因进行了分析,并通过改善带钢表面油膜均匀性、改进退火酸洗工艺,取得了较显著的效果。除2 5~3 0mm厚规格带钢外,基本消除了带钢的条状色差缺陷。
In view of existing linear chromatism on the surface of the cold rolled stainless strip which produced by Zhangjiagang Pohang Stainless Steel Co,Ltd,the causes of its formation were analyzed and some measures were carried out,such as improving the uniformity of oil film on strip surface and reforming pickling processingAs the result,the linear chromatism can be eliminated except 25~30mm gauge strip
出处
《轧钢》
2002年第6期24-26,共3页
Steel Rolling
关键词
不锈钢
冷轧带钢
条状色差
产生原因
改进措施
stainless steel
cold rolled strip
linear chromatism
cause
improvement measures