摘要
青海盐云钾盐有限公司二车间冷分解—正浮选法生产氯化钾工艺存在钾盐分解回收率低、尾盐氯化钾含量高等问题。文章通过流程考察和浮选试验,发现这些问题由工艺生产过程中分解水量过多、浮选时分离效果差、洗涤水量过多等因素导致。根据流程考察和试验结果,分别从分解工序、浮选工序、洗涤过滤工序、干燥包装工序提出合理化建议。
The cold decomposition-positive flotation method of the second workshop of Qinghai Yanyun Potash Co.,Ltd.to produce potassium chloride has problems such as low recovery rate of potassium salt decomposition and high potassium chloride content of tail salt.This article found through process investigation and flotation experiments that these problems are caused by excessive decomposition water during the production process,poor separation efficiency during flotation and excessive washing water volume.According to the process investigation and test results,reasonable suggestions were put forward from the four processes of decomposition process,flotation process,washing and filtration process and drying and packaging process.
作者
刘清
宋宪伟
吴志刚
张守祥
刘星强
赵海平
LIU Qing;SONG Xianwei;WU Zhigang;ZHANG Shouxiang;LIU Xingqiang;ZHAO Haiping(Bluestar Lehigh Engineering Institute Co.,Ltd.,Lianyungang 222000,China;Qinghai Yanyun Potash Co.,Ltd.,Golmud 816000,China)
出处
《盐科学与化工》
2025年第1期18-22,共5页
Journal of Salt Science and Chemical Industry
关键词
钾盐
冷分解
结晶
正浮选
Sylvite
Cold decomposition
Crystallized
Positive flotation