制硫装置解吸塔塔体裂纹形成原因分析

The Analysis of the Cause of Crackles of the Desorber and the Application of the Countermeasure
在线阅读 下载PDF
导出
摘要 通过宏观检查、金相组织检验及裂纹断口观察 ,分析了制硫车间解吸塔 (C - 40 3/ 2 )塔体裂纹产生的原因 。 The cause of crackles of the desorber (C-403/2) is analyzed. There are three reasons. Firstly, the high content of Sulfur (S) and Phosphorus (P) in the steel where by heavily debases the capability of erosion-resistant; secondly, the high-temperature sulfides, that accelerate the erosion; thirdly, the effect of stress-erosion. A countermeasure has been put forward according to the specific condition, which are a new tower built later. A reasonable controlling measure has been put forward, which assures that the manufacture and installation of the new tower meet the technological specification and prevent the occurrence of the similar situation.
作者 肖涤 刘忠友
出处 《石化技术》 CAS 2002年第3期138-141,共4页 Petrochemical Industry Technology
关键词 制硫装置 解吸塔 塔体 裂纹 形成原因 应力腐蚀 热处理 dissolving-absolving tower, stress-erosion, crackle, heat treatment
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部