摘要
对某难处理金矿热压氧化渣进行炭浸氰化试验,考察pH、调浆时间、底炭浓度、氰化钠初始浓度、浸出时间对金浸出率的影响。结果表明,在下述最佳条件下,氰化钠的消耗仅为0.27~0.29kg/t,金浸出率为95.34%:底炭浓度60kg/t、氧化钙用量35kg/t、氰化钠初始浓度1.5kg/t、调浆时间2h、室温浸出2~4h。难处理金矿经过热压氧化预处理后炭浸法提金,具有浸出反应动力学快,浸出率高,氰化钠消耗低的特点。
Residue of refractory gold ore after pressure oxidation pretreatment was leached by carbon-in- leach (CIL). Effects of pH, slurry-mixing time, active carbon concentration, initial concentration of NaCN, and leaching time on gold leaching rate were investigated. The results show that gold leaching rate is 95. 340//00 with NaCN consumption of 0.27~0.29 kg/t under the optimum conditions including active carbon concentration of 60 kg/t, CaO consumption of 35 kg/t, initial concentration of NaCN of 1.5 kg/t, slurry-mixing time of 2 h, and leaching duration of 2-4 h at room temperature. This process has the advantages of fast reaction kinetics, high gold leaching rate, and low consumption of NaCN.
出处
《有色金属(冶炼部分)》
CAS
北大核心
2016年第9期28-30,47,共4页
Nonferrous Metals(Extractive Metallurgy)
基金
广西科学研究与技术开发计划项目(桂科攻14122006-25)
中国有色集团科技计划项目(2014KJJH02)
关键词
难处理金矿
热压氧化
炭浸法(CIL)
refractory gold ore
pressure oxidation
carbon-in-leach process (CIL)