复杂载荷下石油套管破坏实验的关联分析

Correlative Analysis of Casing Destructive Testing under Complicated Loads
在线阅读 下载PDF
导出
摘要 采用关联分析方法对石油套管在复杂载荷下的破坏实验数据进行了关联分析。结果表明 ,外径和壁厚是影响套管径向极限承载能力的 2个主要因素 ;套管外挤压力对套管轴向极限承载能力的影响很大 ;椭圆度仅对均匀外挤压力导致套管破坏有较大影响。 Casing destructive testing data are analyzed correlatively under complicated loads by using a correlative analytical method The result indicates that outside diameter and wall thickness are two key factors influencing the casing radial limit loading capacity, the effect of outside casing squeeze pressure on its axial limit loading capacity is very big, the only effect of ellipticity on casing destruction caused by even outer squeeze pressure is higher
作者 张系斌
出处 《江汉石油学院学报》 CSCD 北大核心 2001年第4期79-80,共2页 Journal of Jianghan Petroleum Institute
关键词 石油套管损坏 径向力 轴向力 承压能力 实验数据 影响因素 关联分析 casing failure radial force axial force pressuring capacity experimental data influencing factor correlative analysis
  • 相关文献

参考文献9

  • 1张百龙 王振华 等.石油套管研究情况概述[J].石油机械,1987,15(4):38-41.
  • 2张百龙 王振华 等.围岩压力下套管承载能力的研究[J].石油机械,1987,15(10):26-33.
  • 3张系斌 王振华 等.套管变形的初步研究[J].石油机械,1987,15(11):32-38.
  • 4王振华 张系斌 等.轴力对套管临界外挤压力影响的研究[J].石油机械,1988,16(2):6-12.
  • 5傅立,灰色系统理论及其应用,1992年,185页
  • 6王振华,石油机械,1988年,16卷,2期,6页
  • 7张百龙,石油机械,1987年,15卷,10期,26页
  • 8张百龙,石油机械,1987年,15卷,4期,38页
  • 9张系斌,石油机械,1987年,15卷,11期,32页

共引文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部