摘要
以实验室的热模拟变形实验和轧制实验为基础 ,依据形变诱导相变理论 ,制定了现场轧制工艺。通过细晶强化和相变强化 ,使普通 SS40 0钢的屈服强度达到了 40 0 MPa,开发出超级 Super- SS40
Based on the thermo mechanical simulation and experimental rolling and the theory of deformation induced transformation, the rolling schedule of industrial trials was worked out The yield strength of SS400 steel was enhanced to 400 MPa and a new super steel named Super SS400 has been developed through refining grain size and phase transformation
出处
《钢铁》
CAS
CSCD
北大核心
2001年第5期39-43,共5页
Iron and Steel