摘要
本文通过测定9种温变(26℃≤T≤530℃)下6542型高速钢和纯铁的穆斯堡尔谱,给出各种温度下实验数据拟合结果和其无反冲因子随温度变化规律,并讨论了高速钢随着温度的提高发生相结构变化的规律。
Mossbauer spectra of both Model 6542 high-speed steel and pure iron have been measured at different temperatures (26℃≤T≤530℃) . The experimental data were fitted and their recoilless factors were obtained. The temprature-phase dependence of 6542 high speed steel is discussed.
出处
《核技术》
CAS
CSCD
北大核心
1991年第4期207-212,共6页
Nuclear Techniques
关键词
高速钢
穆斯堡尔谱
无反冲因子
High-speed steel Mossbauer spectrum Recoilless factor