摘要 以硫脲作为硫源 ,在瓦特浴体系中通过电沉积方法获得Ni S合金电极·系统地讨论了电沉积过程中各工艺条件 (硫脲浓度、电流密度、pH值及温度 )对镀层中S含量的影响 ,确定了硫脲浓度和电流密度为Ni S合金镀层中S含量的主要影响因素 ;以恒电流极化方法测试不同S含量的合金电极的析氢过电位 ,得到了析氢过电位仅为 90mV的非晶态Ni S合金析氢阴极 ;以稳态极化方法测定该电极的稳态极化曲线 ,并通过计算得出其电化学参数 (b,i0 ) ·结果表明 ,该电极具有极高的电化学活性· Nickel sulfur electrode was obtained in typical Watt bath adding thiourea by electrodeposition. The effects of thiourea concentration, current density, temperature and pH value of electrolyte on sulfur content in the deposited nickel sulfur electrode were systematically studied, and the hydrogen evolution overvoltage and electrochemical parameters of nickel sulfur electrode were measured as well. The results indicate that main factors which influence sulfur content in the coatings on the electrode are thiourea concentration and current density, and that the nickel sulfur electrode presentes low hydrogen evolution overvoltage and high electrochemical activity.
作者 韩庆 魏绪钧
出处 《东北大学学报(自然科学版)》 EI CAS CSCD 北大核心 2000年第5期539-542,共4页 Journal of Northeastern University(Natural Science)
基金 国家自然科学基金资助项目! ( 59874 0 11)
关键词 电沉积 析氢阴极 硫脲 电解制氢 镍硫合金 electrodeposit Ni S electrode hydrogen evolution
  • 相关文献

参考文献1

  • 1Wen T C,J Appl Electrochem,1994年,24卷,233页

同被引文献56

引证文献6

二级引证文献41

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部