结合辅料分厂6×155m3白灰竖窑的实际生产情况,分析了1#、2#、3#窑内衬使用高铝砖和粘土砖损毁机理,并提出相应的延长竖窑内衬使用寿命的措施。
The paper analyzes high alumina bricks and clay brick damage mechanism, and puts for- ward the corresponding measures to prolong the service life extension of kiln combined with accessories factory 6 ×155m^3 lime shaft kiln production practice and 1#, 2#, 3# kiln lining using.