摘要
西藏某锑铅选矿厂的脆硫锑铅矿与方铅矿的混合精矿产品有价元素为铅、锑,矿样经活性炭脱药后,对混合精矿进行浮选分离试验,获得了铅品位为72.09%、回收率为50.96%的铅精矿,锑品位为10.89%、回收率为76.67%的锑精矿,实现了铅、锑的有效分离。
The valuable element of a mixed concentrate, composition of galena and jamesonite, in Tibet was lead and antimony. After reagent removal by active carbon, galena concentrate with Pb grade of 72.09% , recovery of 50.96% , and jamesonite concentrate Sb grade of 10.89% , recovery of 76.67% was achieved by whole flotation process.
出处
《现代矿业》
CAS
2013年第10期24-26,共3页
Modern Mining
基金
"十二五"国家科技支撑计划重点项目(编号:2012BAB10B05)
关键词
方铅矿
脆硫锑铅矿
脱药
浮选
Galena, Jamesonite, Dereagent, Flotation