当离心机铸型的温度超过某一范围后,其力学性能大幅降低,在高速旋转下,铸型碎裂的风险也大大提高。通过研究,本文给出了几种常用铸型材料的适用条件及预设温度。对于由相同材质组合的离心铸型,能通过计算最小铸型质量,使铸型温度控制在预设温度以内;对于由不同材质组合的离心铸型,则给出了简化方法。通过控制铸型质量,将铸型温度控制在预设温度以内,不仅能防止铸型处于因力学性能大幅降低而导致碎裂的高风险状态之中,而且还可以延长铸型的使用寿命。
Mechanical properties of casting mould for centrifugal machine will reduce quickly when temperature of casting mould exceeds a certain range, and cataclastic risk will increase greatly when casting mould spin at high speed. The paper presented suitable condition and presetting temperature in several kinds of common mould materials by studying. Temperature of casting mould made of the same materials can be controlled within presetting temperature by calculating mini casting mould mass, simplification technique of presetting temperature for casting mould made of different materials was presented. The temperature for casting mould was controlled within presetting temperature by controlling casting mould mass, the measures can not only prevent casting mould from cataclastic risk, but also extend service life of casting mould.
出处
《铸造》
CAS
CSCD
北大核心
2013年第10期987-990,共4页
Foundry
关键词
离心铸造
离心铸型
铸型预设温度
centrifugal casting
large and middle casting mould
presetting temperature control in casting mould