期刊文献+

牙列重度磨耗患者经热压铸瓷修复后的短期临床评价 被引量:1

Evaluation of IPS e. max Press in the reconstruction of occlusion for the patients with tooth wear
暂未订购
导出
摘要 用IPSe.max Press热压铸瓷对16例牙列重度磨耗患者(共398个牙单位)进行咬合重建。针对口腔具体条件,分别选择贴面、咬合罩面、全瓷冠桥修复,随访6~12个月,参照改良的美国公共卫生署评价标准进行评价,对数据进行非参数统计学分析。390单位修复体成功,成功率97.9%,所有修复体边缘密合、色泽自然、外形协调,在各评价项目均无统计学差异(P〉0.05)。在筛选合适病例的前提下,用IPSe.max Press热压铸瓷为牙列重度磨耗患者进行咬合重建的短期效果良好。 16 patients with 398 dental units of severe dental attrition were rehabilitated by IPS e. max Press for occlusion reconstruction. After 6 -24 months follow-up, patients were satisfied with their prosthesis. Excessive toothwear or prostheseswear were not observed. All pa- tients'temporomandibular joints were in concordant condition. No secondary carries of the treated teeth was found. The proothesis color matched with the nature teeth. The success rate was 97.9% ( P 〉 0.05 ). IPS e. max Press is an effective and reliable treatment for advanced tooth wear.
出处 《实用口腔医学杂志》 CAS CSCD 北大核心 2013年第5期739-740,共2页 Journal of Practical Stomatology
基金 江苏省科技厅临床医学科技专项基金(编号:SBL201230169)
关键词 牙列重度磨耗 咬合重建 IPS e max Press热压铸瓷 Severe dental attrition Occlusal reconstruction IPS e. max Press
  • 相关文献

参考文献8

  • 1Schaefer O, Watts DC, Sigusch BW, et al. Marginal and internal fit of pressed lithium disilicate partial crowns in vitro: A three-dimensional analysis of accuracy and repro- ducibility [ J ]. Dent Mater, 2012, 28 (3) :320 - 326.
  • 2Cvar JF, Ryge G. Reprint of criteria for the clinical evalua- tion of dental restorative materials. 1971 [J]. Clin Oral In- vestig, 2005, 9(4):215-232.
  • 3Etman MK. Confocal examination of subsurface cracking in ceramic materials [ J]. J Prosthodont, 2009,18 ( 7 ) : 550 - 559.
  • 4Stappert CF,Att W, Gerds T, et al. Fracture resistance of different partial-coverage ceramic molar restorations: An in vitro investigation[J ]. J Am Dent Assoc, 2006,137 (4) : 514 - 522.
  • 5Etman MK,Woolfood MJ. Three-year clinical evaluation of two ceramic crown systems: A preliminary study [J ] J Prosthet Dent, 2010,103 ( 2 ) : 80 - 90.
  • 6劳恩(Lawn,B.)著.龚江宏译.脆体固体断裂力学[M].北京:高等教育出版社,2010:14-35.
  • 7张志升,徐勇,苏剑生,刘伟才,肖云.牙科陶瓷材料弯曲强度可靠性和亚临界裂纹扩展研究[J].实用口腔医学杂志,2011,27(3):339-342. 被引量:4
  • 8介艳巧,夏荫培,张修银,吴艳玲.光弹法在双层结构全瓷冠应力分析中的应用[J].实用口腔医学杂志,2011,27(4):441-445. 被引量:5

二级参考文献15

  • 1LI Li-li,WANG Zhong-yi,BAI Zhong-cheng,MAO Yong,GAO Bo,XIN Hai-tao,ZHOU Bing,ZHANG Yong,LIU Bing.Three-dimensional finite element analysis of weakened roots restored with different cements in combination with titanium alloy posts[J].Chinese Medical Journal,2006(4):305-311. 被引量:26
  • 2张志升,刘伟才,苏剑生.牙科陶瓷材料疲劳研究进展[J].中华老年口腔医学杂志,2006,4(1):56-58. 被引量:4
  • 3Bona AD, Anusavice K J, De Hoff PH. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures [J]. Dent Mater,2003,19 ( 7 ) :662 - 669.
  • 4Weibull BW. A statistical distribution function of wide applicability [ J ]. J Appl Mech, 1951,18 ( 3 ) : 293 - 297.
  • 5Seghi RR,Sorensen JA. Retative flexual strength of six new ceramic materials [ J ]. Int J Prosthodont, 1995,8 (4) : 239 - 246.
  • 6Studart AR, Filser F, Kocher P, et al. In vitro lifetime of dental ceramics under cyclic loading in water[ J]. Biomate- rials, 2007, 28(17) :2695-2705.
  • 7Schmitt R, Fett T, Munz D. Cyclic fatigue of zirconia[J]. Fatigue Fract Eng Mater Struct, 1996, 19 (12) : 1411 - 1420.
  • 8Munz D, Fett T. Ceramics : Mechanical properties, failure behaviour, materials selection [ M ]. Berlin: Springer-Verlag, 1999 : 167 - 172.
  • 9Zeng K, Oden A, Rowcliffe D. Flexure tests on dental ceramics [ J ]. Int J Prosthodont, 1996,9 (5) :434 - 439.
  • 10Tanake T. Fatigue crack growth of silicon nitride with crack wedging by fine fragment [ J ]. Fatigue Fract Engng Mater Struct, 1992, 15(7): 643-653.

共引文献7

同被引文献2

引证文献1

二级引证文献32

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部