摘要
分析了钩尾宽框后堵折断故障的主要原因,提出了改进意见,以防止事故的发生,保证行车安全。
出处
《西铁科技》
2000年第4期51-52,50,共3页
Xi'an Railway Technology
同被引文献13
-
1А.В.Богданович,张孝仁.自动车钩用的20ГСФТЛ号钢的疲劳强度综合特性的试验研究[J].国外机车车辆工艺,1993(2):25-29. 被引量:1
-
2严隽耄.车辆工程[M].北京:中国铁道出版社,2004..
-
3陈建敏,周惠娣.磨损失效与摩擦学新材料[c].第三次全国机电装备失效分析预测预防战略研讨会论文集,1998:73-80.
-
4Warke W R. Seeking the basic cause of gas turbine hot section failure [ A ]. Proceeding of International Conference on Failure Analysis and Prevention, 1995:551 - 560.
-
5Toshim K. Evaluation of dynamic fracture toughness by instrumented impact test [ A ]. Proceeding of International Conference on Failure Analysis and Prevention,1995:38 -46.
-
6Berns H, Broeckmann C. Fracture mechanisms in particle reinforced metal matrix composites [ A ]. Proceeding of International Conference on Failure Analysis and Prevention, 1995:219 - 224.
-
7卢桐森.新造C50型后从板座弯曲变形原凶分析[J].铁道车辆,1979(3):38-40.
-
8E1-Sibaie M. Recent advancements in buff and draft testing techniques [ C ]. Fifth International Heavy Haul Conference, Beijing, 1993 : 115 - 119.
-
9韩培德,武晓雷,孙艳明.铁基合金激光熔覆组织及其冲击磨损性能[J].材料科学与工艺,1999,7(2):22-26. 被引量:15
-
10田武岭,张建武,管艳华,姜岩.重载货车17号车钩疲劳寿命试验与可靠性预测[J].机械设计与研究,2012,28(3):115-118. 被引量:4
二级引证文献3
-
1李翔,吴毅,尹鸿祥,张关震,张恒.铁路货车补焊前从板断裂分析[J].兵器材料科学与工程,2021,44(2):54-57.
-
2李辉,蔡建伟,王超会.新型铁路货车车钩用钢的磨损性能研究[J].热加工工艺,2022,51(2):153-155. 被引量:2
-
3谢猛.铁路货车钩缓装置检修设备自动化研究[J].中国新技术新产品,2022(12):93-95. 被引量:1
-
1徐荣波.铁路货车高磨合成闸瓦折断故障的分析和建议[J].西铁科技,2014,0(4):8-9.
-
2熊树林,迟胜超.减速顶壳体螺栓发生折断故障原因分析及应对措施[J].减速顶与调速技术,2008(1):4-7.
-
3段建奎,柳拥军.长大货物列车钩舌折断的原因分析[J].铁道车辆,2007,45(11):43-43.
-
4张雨天.交叉杆安全链卡子折断故障多发的原因[J].铁道机车车辆,2005,25(4):62-62.
-
5李涛.浅谈接触网支柱折断故障预抢方案[J].西铁科技,2008(2):27-29.
-
6崔兴,亓仲印.上海日野P11C-UJ型发动机气门折断故障的排除[J].汽车维护与修理,2011(11):35-35.
-
7郑耀军,陈有成.16、17型车钩钩提杆折断故障探讨[J].铁道车辆,2015,53(1):44-44. 被引量:1
-
8樊晓磊.铁路货车人力制动机链条折断故障维修材料设计建议[J].河南科技,2014,33(4):75-76.
-
9断轨动态监测装置[J].中国铁路,2006(2):72-72.
-
10张印江.挤切销非挤切折断故障的预防[J].铁道通信信号,1992(2):27-28.