期刊文献+

海水润滑条件下40Cr钢的冲击磨损实验研究 被引量:3

A Study on Impact Wear of 40Cr Steel with Briny Lubrication
在线阅读 下载PDF
导出
摘要 使用冲击磨损试验机、扫描电镜及表面形貌仪研究冲击载荷作用下40Cr钢在海水润滑工况下的表面损伤行为。结果发现,冲击使材料表面发生了塑性变形和磨损,塑性变形存在于冲击的每一阶段;冲击凹坑深度及体积随冲击次数的增加呈增大趋势;相比干接触条件,使用海水润滑可有效抑制冲击磨损,但会对冲击凹坑表面造成一定的腐蚀,并且该腐蚀程度随载荷的增加而增强;相同冲击次数条件下,海水润滑时的冲击凹坑深度和体积大于BS05润滑油润滑时的凹坑深度和体积。 The damage behaviors of 40Cr steel with briny lubrication were Studied using a self-made impact test rig, the SEM and the surface topography instrument. The results indicate that the surface of the material has undergone plastic de- formation and wear, and plastic deformation appears in each stage of impact. With the impact times increasing, the depth and volume of the impact dent are increased. Compared with the dry condition, the sea water can restrain impact wear effectively while cause the dent damaged by Corrosion. With impact load increasing, the degree of corrosion is enhanced. Under same impacting time, the larger depth and volume of impact dent are produced under briny lubrication compared with under BS05 oil lubrication.
出处 《润滑与密封》 CAS CSCD 北大核心 2013年第6期43-48,52,共7页 Lubrication Engineering
基金 国家自然科学基金项目(51275253) 国家973子课题(2011CB706602-16)
关键词 冲击磨损 40CR钢 海水润滑 塑性变形 impact wear 40Ct steel briny lubrication plastic deformation
  • 相关文献

参考文献10

  • 1Slatter T,Lewis R,Jones A H. The influence of cryogenic processing on wear on the impact wear resistance of low carbon steel and lamellar graphite cast iron [ J ]. Wear, 2011,271 : 1481 - 1489.
  • 2Sundstrom A , Rendona J, Olsson M. Wear behaviour of some low alloyed steels under combined impact/abrasion contact conditions [ J ]. Wear, 2001,250 : 744 - 754.
  • 3Zhang Guoshang,Xing Jiandong, Gao Yimin. Impact wear resistance of WC/Had field steel composite and its interfacial characterisitics [ J ]. Wear,2006,260:728 - 734.
  • 4Mann b S. High-energy particle impact wear resistance of hard coating and their application in hydroturbines [ J ]. Wear, 2000, 237 : 140 - 146.
  • 5Iwai Y,Honda T,Yamada H,Matsubara T,et al. Evaluation of wear resistance of thin hard coatings by a new solid particle impact test [ J ]. Wear,2001,251:861 - 867.
  • 6薛峰,周仲荣.AZ91D镁合金在水介质下的冲击磨损特性研究[J].机械,2008,35(2):69-72. 被引量:5
  • 7Du Xiaodong,Wang Jiaqing, Sun Guodong,et al. Effect of composition on impact-wear behavior of alloyed liner steels in corrosive condition [J]. Materials Science and Engineering ,2008,477:277 - 281.
  • 8石成霞,王静,陈凡秀,李宏升.重冲击载荷作用下硬铝合金的损伤行为研究[J].润滑与密封,2011,36(2):38-44. 被引量:7
  • 9卢磊磊,王静.表面具有焊层的45#钢冲击磨损的实验研究[J].润滑与密封,2012,37(5):43-47. 被引量:6
  • 10吴海荣,毕秦岭,杨军,刘维民.巴氏合金ZChSnSb 8-8海水环境下的摩擦学行为研究[J].摩擦学学报,2011,31(3):271-277. 被引量:12

二级参考文献46

共引文献22

同被引文献24

引证文献3

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部