期刊文献+

铜质接地网材料腐蚀特性 被引量:3

Corrosion Performance of Copper Grounding Material
在线阅读 下载PDF
导出
摘要 采用极化曲线和电化学阻抗谱研究了铜质接地网材料在1∶1水土混合液中的腐蚀行为;通过实验室埋片试验和变电站现场测试,研究了铜质接地网材料在土壤介质的腐蚀特性。结果表明,铜试样在弱酸性和弱碱性土壤中没有发生明显的局部腐蚀,且均匀腐蚀速率较小,以目前变电站常用的TJ-240硬铜绞线计,铜接地网材料满足设计使用寿命要求。 The corrosion behavior of copper grounding material was studied by polarization curves and EIS under the condition of soil : water = 1 : 1. In addition, the corrosion performance of copper grounding material in a variety of soil media was studied using laboratory corrosion tests and substation field tests. The results showed that copper samples exhibited no obvious localized corrosion in weak acidic and weak alkalic soils, and its uniform corrosion rate was small. Therefore, the common used TJ-240 copper stranded wire is able to fulfill the requirements of design service life.
出处 《腐蚀与防护》 CAS 北大核心 2013年第6期507-510,541,共5页 Corrosion & Protection
关键词 接地网 极化曲线 电化学阻抗谱 腐蚀特性 copper grounding grid polarization curve electrochemical impendence spectroscopy corrosion performance
  • 相关文献

参考文献4

二级参考文献2

  • 1贝克曼WV,施文克W.阴极保护手册电化学保护的理论与实践[M].北京:化学工业出版社,2005.
  • 2许崇武,胡学文,郑敏聪.接地网防蚀金属材料性能试验研究[C].火电厂水处理技术研讨会交流资料之二.重庆:中国电机工程学会,2003.

共引文献32

同被引文献35

引证文献3

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部