期刊文献+

某低品位钼矿浮选工艺研究 被引量:7

Research on Floatation Technology of a Low Grade Molybdenum Ore
在线阅读 下载PDF
导出
摘要 某钼矿含钼0.045%,含硫3.16%,钼主要以独立的辉钼矿形式存在,其他硫矿物以黄铁矿、黄铜矿为主,脉石矿物主要为石英、云母、长石。辉钼矿以中细粒嵌布为主,其粒度分布范围较宽,与黄铁矿等硫化矿关系比较紧密。采用粗磨浮钼—粗精矿细磨精选—钼粗选尾矿选硫的工艺流程,获得了合格的钼精矿,并综合回收硫。浮选闭路试验指标为:钼精矿品位45.13%、钼回收率83.97%,硫精矿品位51.06%、硫回收率95.36%。 A molybdenum ore contains 0.045% Mo and 3.16% S, in which molybdenite supplies Mo overwhelmingly, pyrite and chaleopyrite contribute other S mainly. Quartz, mica and feldspar are the main gangue minerals. Molybdenite ore with wide particle size distribution is embed in other sulfide minerals, and characterized by a fine-grained dissemination characteristics. A process consisting of preferential Mo flotation, rough Mo-eoncentrate regrinding and sulfur dressing of rough Mo-tailings is used in the test. In the closed circuit test, molybdenum concentrate can be acquired with Mo content 45.13% and recovery 83.97%, and sulphur concentrate with S content 51.06% and recovery 95.36%.
出处 《有色金属(选矿部分)》 CAS 北大核心 2013年第1期35-39,共5页 Nonferrous Metals(Mineral Processing Section)
关键词 低品位钼矿 粗磨 综合回收 low-grade molybdenum ore coarse grinding comprehensive recovery
  • 相关文献

参考文献4

二级参考文献18

共引文献15

同被引文献43

引证文献7

二级引证文献16

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部