期刊文献+

降低超低碳钢冷轧产品夹杂的生产控制实践 被引量:3

Producing and Controlling Practice of Reducing Inclusion in Super Low Carbon Steel
在线阅读 下载PDF
导出
摘要 济钢在生产超低碳钢冷轧产品的过程中,产生大量的夹杂物缺陷造成的冷轧次、废品损失,夹杂缺陷改判率最高时达到1.5%。通过分析夹杂物的来源及形成机理,制定了相应的改进措施,减少了夹杂缺陷,超低碳钢冷轧产品夹杂的改判率降至0.6%以下。 In the production course of cold-rolling products of super low carbon steel in Jinan Steel, a large number of inclusion defects appeared, which resulted in cold-rolling sub-standard products and waste products. The largest judgment-changing rate for inclusions reached 1.5%. Through analyzing the source and forming mechanism of the inclusions, corresponding improvement measures were taken, reducing the inclusion defects. The judgment-changing rate for inclusions of cold-rolling products of super low carbon steel is decreased to 0.6% below.
出处 《山东冶金》 CAS 2012年第5期22-24,共3页 Shandong Metallurgy
关键词 超低碳钢 冷轧 夹杂物 改判率 super low carbon steel cold-rolling inclusion judgment-changing rate
  • 相关文献

参考文献2

二级参考文献4

共引文献6

同被引文献30

引证文献3

二级引证文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部