摘要 超细晶硬质合金是WC晶粒度≤0.5μm的硬质合金,这类合金具有高强度和高硬度的优异性能。目前由超细晶硬质合金制备的高效刀具已经广泛用于航空航天、核能、汽车、发电设备、新能源和电子通讯等现代制造业。主要对中国超细晶硬质合金原料(例如超细碳化钨粉、钴粉、复合粉)和超细晶硬质合金制备技术、性能及表征方法作了系统的阐述。最后对超细晶硬质合金制备技术进行了展望。 The sintered WC-Co with uhrafine grain sizes ( 〈 0. 5 rim) is called ultrafine cemented carbide, which pos- sesses optimized properties such as hardness and strength. Efficient tools prepared by uhrafine cemented carbides have been used in aerospace, nuclear energy, automotive, generating equipment, new energy and other fields of electronic communications. The development of uhrafine cemented carbides and raw materials was systematically introduced and reviewed, mainly in aspects of the preparation, property and characterization of uhrafine tungsten carbide powder, ultrafine cobalt powder, WC-Co composite powder and ultrafine cemented carbides in China. Prospects on technology of the ultra-fine cemented carbide were discussed finally.
出处 《中国材料进展》 CAS CSCD 2012年第4期39-46,共8页 Materials China
基金 国家科技重大专项(20092x04012-032) 国家科技支撑计划资助项目(2007BAE05B02)
关键词 超细晶 硬质合金 碳化钨 钴粉 球形度 uhrafine crystal cemented carbide tungsten carbide cobalt powder sphericity
  • 相关文献

参考文献27

  • 1Gille G, Szesny B, Dreyer K, et al. Submicron and Ultrafine Grained Hardmetals for Microdrills and Metal Cutting Inserts[ J ]. International Journal of Refractory Metals and Hard Materials, 2002, 20(1): 3-22.
  • 2Kai E, Shigeyuki H, Sho T, et al. Fabrication and Cutting Performance of Cemented Tungsten Carbide Micro-cutting Tools [ J ].Precision Engineering, 2011, 35 ( 4 ) : 547 - 553.
  • 3工具行业“十二五”发展规划建议草案(切削刀具部分)(一)[J].工具展望,2011(2):2-9. 被引量:2
  • 4Miyake M, Hara A, Sho T. Direct Production of WC from WO3 by Using Two Rotary Carburization Furnaces [ J ]. Journal of Japan Society of Powder and Powder Metallurgy, 1979, 26 ( 3 ) : 90 -95.
  • 5Asada N, Yamamoto Y, Shimatani K, et al. Particle Size of Fine Grain WC by the Continuous Direct Carburizing Process[ J]. Metal Powder Report, 1990, 45( 1 ) : 60 -64.
  • 6Conner C L. Dow Finds Cost Effective Route to Fine WC Powders [J]. Metal Powder Report, 1997, 52(12) : 27 - 31.
  • 7Wu Chonghu. Preparation of Ultrafine Tungsten Powders by In-Situ Reduction of Nano-Needle Violet Tungsten Oxide[J]. International Journal of Refractory Metals and Hard Materials. 2011, 29 (6) : 686 - 691.
  • 8吴冲浒.钨粉碳化过程中反应物装舟量对碳化速率和能耗的影响[J].粉末冶金材料科学与工程,2010,15(6):597-600. 被引量:4
  • 9Upadhyaya G S. The Materials Science of Cemented Carbides an Overview [ J ]. Materials and Design, 2001, 22 ( 6 ) : 483 - 489.
  • 10张太全.分解还原法制备超细球形钴粉的过程机理[J].粉末冶金材料科学与工程,2010,15(6):593-596. 被引量:4

二级参考文献113

共引文献90

同被引文献384

引证文献37

二级引证文献127

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部