摘要
通过不同的强磁精矿配比试验进行烧结,使烧结矿性能指标发生变化,我们分析其变化规律,找到能指导实际生产的配比。即强磁精矿配比应控制在10%~30%之间,并能起到调节烧结矿中SiO2的作用,从而科学地利用了强磁精矿。
With different proportioning of ferromagnetic mines,the performance indices of agglomerate will change.In the paper,the proportioning which could guide the actual productions is found out by analyzing the law of changes,that is the proportioning of ferromagnetic mines should be controlled between 10% and 30% to adjust SiO2 in agglomerate so that the ferromagnetic mines are used scientifically.
出处
《包钢科技》
2012年第1期3-5,共3页
Science & Technology of Baotou Steel
关键词
强磁精矿
配比
试验研究
ferromagnetic mines
proportioning
experimental study