地下室混凝土连续外墙裂缝与渗漏将直接影响到建筑物结构的整体性、使用性和耐久性。主要探讨分析了造成地下室混凝土连续外墙裂缝的主要因素,并针对这些因素给出一些裂缝预防措施和裂缝处理方法。
Continuous concrete wall of basement crack and leakage will directly affect on the structural integrity of the building, usability and durability.This article has focused on analysis of main factors contributing to continuous concrete wall of basement crack and prevention measures against these factors giving some cracks and crack treatment methods.