摘要 600 MW机组的螺旋水冷壁爆管原因较难查找,主要是因为影响爆管的因素较多,经过螺旋后无法直观判断对应的下集箱出口及上集箱进口位置。通过对爆口管进行金相、化学、机械性能试验分析,得出超温是水冷壁爆管的主要原因并给出了预防措施,供爆管分析时参考。 Due to that there are many factors influencing on the tube cracking fault,and it can not judge the positions on low header outlet and upper header outlet corresponding with the spiraled tubes intuitively,it is difficult to find the reason of tube cracking of spiral water wall in a 600 MW unit.Based on the metallographic analysis,the chemical analysis and the mechanical test of the cracked tube,it was found that the main reason of the water wall tube cracking is overtemperature,and the preventive measures were given,which provides certain reference for tube cracking analysis.
作者 翁金钰
出处 《华电技术》 CAS 2012年第2期13-15,21,共4页 HUADIAN TECHNOLOGY
关键词 螺旋水冷壁 爆管 超温 砸伤 原因分析 预防措施 spiral type water wall tube cracking overtemperature hurt reason analysis preventive measures
  • 相关文献

参考文献2

二级参考文献3

  • 1GB 5310-20HD8,高压锅炉用无缝铜锈钢管[S].
  • 2Steve R,Paterson Terry W.过热器与再热器管蠕变损伤和剩余寿命和评估[C]∥超役服役机组剩余寿命评估和延寿报告论文集.西安:西安热工研究院,1993.
  • 3马士林,王金瑞,王金新,等.热工技术手册[M].北京:水利电力出版社,1989.

共引文献6

同被引文献30

引证文献9

二级引证文献26

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部