期刊文献+

ICP-AES法测定氧化铁皮中铅、铬、镉 被引量:1

Determination of Pb, Cr and Cd in mill scale by inductively coupled plasma atomic emission spectrometry
在线阅读 下载PDF
导出
摘要 建立了电感耦合等离子体原子发射光谱法测定氧化铁皮中铅、铬、镉的新方法。样品采用盐酸分解,以高纯铁进行基体匹配。铅、铬、镉的检出限分别0.0008%、0.00012%、0.00008%,最大相对标准偏差为8.33%,方法回收率介于92.0%-110%之间。 A new method has been developed for the determination of Pb,Cr and Cd in mill scale by inductively coupled plasma-atomic emission spectrometry(ICP-AES).The samples were digested by HCl(1+1)and determined by ICP-AES with with matrix matching.The detection limits of the method for Pb,Cr and Cd were 0.0008%,0.00012% and 0.00008%,respectively,and the maxium RSD was 8.33%,and the recovery of the method was in the range of 92.0% to 110%.
出处 《福建分析测试》 CAS 2011年第6期54-56,共3页 Fujian Analysis & Testing
基金 国家质检总局课题资助(2010IK033)
关键词 氧化铁皮 ICP-AES mill scale lead chromium cadmium ICP-AES
  • 相关文献

参考文献6

二级参考文献38

  • 1吴祝民.热轧带钢氧化铁皮的成因及对策[J].轧钢,2007,24(3):56-58. 被引量:79
  • 2陈世朴.金属电子显微分析[M].北京:机械工业出版社,1986.87.
  • 3Tominaga Jiro, Wakimoto Kin-ya. Manufacture of wire rods with good descaling property[J]. Transactions ISIJ, 1982, 22: 646-656.
  • 4Bhattacharya R, Jha G. Influence of cooling rate on the structure and formation of oxide scale in low carbon steel wire rods during hot rolling[J]. Surface and Coating Technology, 2006,201 : 526-532.
  • 5Chen R Y, Yuen W Y D. Review of the high-temperature oxidation of Iron and carbon steels in air or oxygen[J]. Oxidation of Metals, 2003, 59 (5/6): 433-468.
  • 6Chen R Y, Yuen W Y D. Oxide-scale structures formed on commercial hot-rolled steel strip and their formation mechanisms[J]. Oxidation of Metals, 2001, 56 (1/2):89-118.
  • 7Chen R Y, Yuen W Y D. A study of the structure of hot-rolled steel strip by simulated coiling and cooling [J]. Oxidation of Metals, 2000, 53(5/6):539-560.
  • 8Sun Weihua, Tieu A K. High temperature oxide scale characteristic of low carbon steel in hot rolling [J]. Journal of Materials Processing Technology, 2004, 155/156 : 1307-1312.
  • 9Torresa M, Colas R. A Model for Heat Conduction Through the Oxide Layer of Steel During Hot Rolling [J]. Journal of Materials Processing Technology, 2000,105(3) : 1483.
  • 10Chen R Y, Yuen W Y D. Review of the High-Temperature Oxidation of Iron and Carbon Steels in Air or Oxygen[J]. Oxidation of Metals, 2003,59(4) :433.

共引文献77

同被引文献5

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部