期刊文献+

高牢度皮革涂饰剂FS-001的研制 被引量:1

Preparation of Leather Coating Agent FS-001 with High Fastness
在线阅读 下载PDF
导出
摘要 介绍了一种乳液聚合方法。通过种子乳液聚合,调整单体比例,引发剂和乳化剂的品种及数量,确定当丙烯酸丁酯和苯乙烯占单体总量的90%~94%,功能单体N-羟甲基丙烯酰胺和丙烯酸羟乙酯占单体总量的2.5%~4.5%,引发剂用量占单体重量的0.9%,阴、非离子乳化剂比例为1∶3,乳化剂总量为单体总量2%,丙烯酸用量为单体总量的3%~4%时,合成的皮革涂饰剂FS-001牢度高,手感好,柔软丰满,具有良好的市场应用前景。 In this article,one kind of emulsion polymerizing method was introduced.By means of seed emulsion polymerizing and adjusting monomer proportion,kind and quantity of initiator and emulsifier,leather coating agent FS-001 with high fastness,good handle,excellent elasticity and good market prospect was synthesized when butyl acrylate and styrene monomer accounted for 90%~94%,functional monomer N-methylol acrylamide and HEMA monomer accounted for 2.5%~4.5%,Initiator accounted for 0.9%,emulsifiers(negative-ionic∶non-ionic =1∶3) accounted for 2% and acrylic monomers accounted for 3% ~4% of total monomer weight.
出处 《皮革与化工》 CAS 2011年第5期12-14,共3页 Leather And Chemicals
关键词 皮革涂饰剂 乳液聚合 种子乳液 leather coating agent emulsion polymerization seed emulsion
  • 相关文献

参考文献2

  • 1(日)大森英三.功能性丙烯酸树脂[M].北京:化学工业出版社,1995.
  • 2复旦大学化学系高分子教研室编.高分子实验技术[M].上海:复旦大学出版社,1983.

共引文献1

同被引文献3

引证文献1

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部