摘要 含钛微合金钢普遍存在钢水可浇性不高,水口易堵塞的问题。综述了国内外铝钛镇静钢的发展和研究现状,分析了铝钛镇静钢脱氧特征,总结了不同脱氧工艺和钢水二次氧化对钢中夹杂物特征的影响,并重点分析了铝钛镇静钢水口结瘤成因及预防措施,以期为提高铝钛镇静钢钢水可浇性和产品质量提供借鉴作用。 Ti-bearing Al-killed steel always present an inferior castability, and a serious nozzle clogging. In this present paper, the research status on about Ti-bearing Al-killed steel was discussed synthetically, feature and behaviors orAl or Ti deoxidation was analyzed. The effect of different deoxidation technology and reoxidation of steel on the inclusions characteristics was summarized, reasons and some preventive measures of nozzle clogging were analyzed, which will be provided some ideas to improve the castability and quality of Ti-bearing Al-killed steel.
出处 《工业加热》 CAS 2011年第4期60-63,共4页 Industrial Heating
基金 国家自然科学基金资助项目(50904017) 教育部基本科研业务费项目(N100402016)
关键词 夹杂物 钛铝脱氧 二次氧化 水口结瘤 inclusions Ti/Al deoxidation reoxidation nozzle clogging
  • 相关文献

参考文献18

  • 1刘中柱,桑原守.氧化物冶金技术的最新进展及其实践[J].炼钢,2007,23(3):7-13. 被引量:64
  • 2亓显玲.洁净钢新技术与高品质钢的生产[J].山东冶金,2009,31(1):5-8. 被引量:8
  • 3赵新凯,李刚利,刘西峰,鞠伟.冷轧低碳铝镇静钢表面起皮缺陷成因分析[J].物理测试,2009,27(5):49-53. 被引量:9
  • 4KANG Y, THUNMAN M, Du S C, et al. Aluminum Deoxidation Equilibrium of Molten Iron-Aluminum Alloy with Wide Aluminum Composition Range at 1873 K [J]. ISIJ International, 2009, 49 (10): 1483-1489.
  • 5PAK J J, JO J O, KIM S I, et al. Thermodynamics of Titanium and Oxygen Dissolved in Liquid Iron Equilibrated with Titanium Oxides [J]. ISIJ International, 2007, 47 (1) : 16-24.
  • 6WASAI K, MUKAI K, MIYANAGA A. Observation of Inclusion in Aluminum Deoxidized Iron [J]. ISIJ International, 2002, 42 (5): 459-466.
  • 7DEKKERS R, BLANPAIN B, WOLLANTS P, et al. A Morphological Comparison between Inclusions in Aluminum Killed Steels and Deposits in Submerged Entry Nozzle [J]. Steel Research, 2003, 74 (6): 351-355.
  • 8SUN M K, JUNG I H, LEE H G. Morphology and Chemistry of Oxide Inclusions After A1 and Ti Complex De-oxidation [J]. Metals and Materials Intemational, 2008, 14 (6): 791-798.
  • 9KIKUCHI N, NABESHIMA S, KISHIMOTO Y, et al. Effect of Ti De-oxidation on Solidification and Postsolidification Microstructure in Low Carbon High Manganese Steel [J]. ISIJ International, 2007, 47 (9): 1255-1264.
  • 10KIKUCHI N, NABESHIMA S, KISHIMOTO Y, et al. Micro-structure Refinement in Low Carbon High Manganese Steels through Ti-deoxidation-Inclusion Precipitation and Solidification Structure [J]. ISIJ Intemational, 2008, 48 (7): 934-943.

二级参考文献28

共引文献78

同被引文献176

引证文献14

二级引证文献70

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部