30CrMnSiNi2A 钢Ms 点以上采用等温淬火工艺, 其强度指标随等温温度升高而降低, 且低于淬火200℃回火的指标值,而塑性、韧性指标相对于淬火200℃回火有明显提高,硬度稍有降低。
Being equal temperature quenched above Ms point, 30CrMnSiNi2A steel's strength targets descend along with the rising of temperature and even be lower than the targets of quenching and 200℃ tempering But its plasticity and toughness targets are evidently rising more than the targets of quenching and 200℃ tempering, its hardness are a little lower 30CrMnSiNi2A steel obtains the best group of the performances by equal temperature quenching from 340℃
出处
《山西机械》
1999年第4期13-15,共3页
Shaanxi Machinery
关键词
等温淬火
性能指标
超高强度钢
CrMnSiNi2A steel
equal temperature quenching
performance target