采煤机行走轮失效分析及改进方法 被引量:12

Analysis on Failure and Improved Method of Shearer Wheel
原文传递
导出
摘要 采煤机行走轮是行走装置的执行机构,属于易损件。主要失效形式为磨损、塑性变形、齿尖断裂等。对已失效的行走轮进行物理金相检验,并对行走轮材料(18Cr2Ni4WA)的金相组织、硬度进行分析,总结了行走轮失效机理。根据失效机理对18Cr2Ni4WA的热处理工艺提出改进,或者更换行走轮材料,选用强度、耐磨性更高的Cr12MoV,以提高齿轨轮的使用寿命。 The shearer wheel belong to easily damaged parts is walking the actuator unit.Major failure modes is wear and plastic deformation,causing faults,etc.Physical metallographic examination be done on the damaged wheel,and do analysis of the microstructure and hardness of the material of shearer wheel and also summarize failure mechanism.According to the failure mechanism,there are measures to improve process of heat treatment of 18Cr2Ni4WA,or to replace the material of wheel,select Cr12MoV higher strength and wear resistance in order to improve the service life of shearer's wheel.
出处 《煤矿机械》 北大核心 2011年第5期167-168,共2页 Coal Mine Machinery
关键词 采煤机 18CR2NI4WA 热处理 金相组织 CR12MOV shearer 18Cr2Ni4WA heat treatment microstructure Cr12MoV
  • 相关文献

参考文献4

二级参考文献11

  • 1林健.18Cr2Ni4WA钢齿轮的热处理[J].铸锻热(热处理实践),1995(2):39-42. 被引量:1
  • 2周广宏,丁红燕.改进预处理工艺 提高模具寿命[J].机械工人(热加工),1996,20(6):13-14. 被引量:1
  • 3王豫.减少18Cr2Ni4W钢残余奥氏体量的热处理工艺[J].华东冶金学院学报,1997,14(2):104-109. 被引量:2
  • 4崔昆.钢铁材料及有色金属材料[M].机械工业出版社,1984..
  • 5王运炎.金属材料与热处理[M].北京:机械工业出版社,1987..
  • 6樊东黎.热处理技术数据手册[M].北京:机械工业出版社,2001.470.
  • 7王广生.金属热处理缺陷分析及案例[M].北京:机械工业出版社,2002..
  • 8上海机械工艺研究所编.金相分析技术[M].上海:上海科学技术文献出版社,1987:484-501.
  • 9李钟晓 张建华.金相组织对齿轮性能的影响.拖拉机,1983,(2):31-31.
  • 10刘云旭.金属热处殚原理[M].北京:机械化工业出版社,1985:213-227.

共引文献51

同被引文献69

引证文献12

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部