摘要
本文研究了不同细度滑石粉填充HDPE体系的力学性能。结果表明;随着滑石粉细度的增加,填充HDPE的拉伸强度和拉伸模量提高了,经偶联剂处理后的滑石粉的填充效果,明显优于未处理的。
This article studied the mechanical performance in HEPE system filled with different talc fineness. The result indicated that the tensile strength and modulus of HDPE filled system is raised with the fineness raising, the effect of filled talc treated by coupling agent is much better than the non-treated, and in which the effect of filled with 2500 mesh talc is the best.