1前言应力腐蚀裂缝至今仍然是焊制容器失效的重要原因之一。为防止应力腐蚀裂缝,通常采用焊后热处理,局部焊后热处理时,主要控制参数是:均热,加热和保温区的宽度。均热区应达到所要求的温度以及容许的温差范围,且不得超过规定的最高温度,它包括焊缝,热影响区以及...
Abstract A series of different local PWHT conditions are studied to find the critical heated widths based on creep FEM analysis and it is found that a heated width of 2 5rt on either side of welds seems reasonable.