摘要 目的探讨氧化铝渗透陶瓷作为全瓷修复体底瓷的修复效果,为临床推广应用提供参考。方法 61例门诊患者,修复体159件,其中上颌98件,下颌61件。前牙全冠132个,后牙全冠27个。通过12~24个月的观察,采用美国加利福尼亚牙科学会的质量评价体系对氧化铝渗透陶瓷作为底瓷所做的前、后牙全冠修复进行临床效果评价。结果对61例患者159颗全冠的临床观察结果表明,氧化铝渗透陶瓷作为底瓷所制作的全瓷修复体具有良好的的边缘密合性,色泽稳定,强度高,其失败率为1.25%,效果满意。结论氧化铝渗透陶瓷作为底瓷的全瓷冠修复是一种效果良好的全瓷修复方式。 Objective To observe the clinical effects of all-ceramic crown using glass-infiltrated alumina core ceramic.Methods A total of 159 crown(98 maxillary and 61 mandibular prostheses)made with glass-infiltrated alumina core ceramic were examined in 61 patients.There were 132 anterior tooth crowns and 27 posterior tooth crowns.Surface,color,anatomic form,and marginal integrity of restorations were assessed at 1 year,1 year and a half,2 years after cementation with the California Dental Association(CDA)quality assessment system.Results It showed that the marginal fitness,color stability and strength of crowns were considered to be satisfactory.Only 1.25 % were not acceptable.Conclusion It is possible to construct excellent all-ceramic prostheses with the glass-infiltrated alumina core ceramic system.
出处 《口腔医学》 CAS 2010年第5期295-297,共3页 Stomatology
关键词 氧化铝渗透陶瓷 全瓷修复 全冠 glass-infiltrated alumina ceramic all-ceramic restorations crown
  • 相关文献

参考文献8

二级参考文献18

  • 1Yoshinari M Kim S 等.Properties of glass infiltrated alumina porcelain (Japanese)[J].齿科材料器械,1994,13(2):170-175.
  • 2万乾炳.一种新型的全瓷修复体——In-Ceram[J].国外医学(口腔医学分册),1997,24(1):3-6. 被引量:12
  • 3Thompson GA. Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite. Dent Mater, 2000,16(4):235-243.
  • 4Bhamra G, Palin WM, Fleming GJ. The effect of surface roughness on the flexure strength of an alumina reinforced all-ceramic crown material. J Dent, 2002,30(4):153-160.
  • 5Fleming GJ, Nolan L, Harris JJ. The in-vitro clinical failure of all-ceramic crowns and the connector area of fixed partial dentures: the influence of interracial surface roughness. J Dent, 2005;33(5):405-412.
  • 6Rowe A, Asgar K. Thermal studies on porcelain substrate metals. J Dent Res, 1976,55:505-506.
  • 7Coffey JP, Anusavice KJ, DeHoff PH, et al. Influence of contraction mismatch and cooling rate on flexural failure of PFM systems. J Dent Res,1988;67(1):61-65.
  • 8Schmid M, Fischer J, Hoffmann C, et al. Chemical and thermal compatibility of all-ceramic systems. Deutsche Zahnarztliche Zeitschrift, 1990,45(8):505-506.
  • 9Anonymous. Porcelain-metal alloy compatibility: criteria and test methods. J Am Dent Assoc, 1981;102(1):71-72.
  • 10Isgro G, Kleverlaan CJ, Wang H, et al. Thermal dimensional behavior of dental ceramics. Biomaterials, 2004,25(12):2447-2453.

共引文献17

同被引文献30

  • 1焦永峰,赵磊.生物陶瓷材料的研究进展[J].江苏陶瓷,2008,41(2):7-9. 被引量:5
  • 2邵聆,施斌.生物活性玻璃在口腔种植中应用的研究进展[J].中华老年口腔医学杂志,2004,2(4):237-239. 被引量:2
  • 3袁捷,祝联,王敏,崔磊,刘伟,曹谊林.自体骨髓基质干细胞-珊瑚羟基磷灰石修复下颌骨节段缺损的实验研究[J].中华口腔医学杂志,2006,41(2):94-97. 被引量:28
  • 4程晓兵,马秦,侯锐,杨耀武,敖建华,毛天球.三维多孔β-磷酸三钙修复下颌骨节段性缺损的生物力学分析[J].临床口腔医学杂志,2007,23(8):469-472. 被引量:3
  • 5Kosmac T. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics [J]. Journal of the European Ceramic Society,2008, 28(5):1085-1090.
  • 6Pittayachawan P., A. Mcdonald, A. Petrie, J. Knowles. The biaxial flexural strength and fatigue property of Lava? Y-TZP dental ceramic [J].Dental Materials,2007,23(8):1018-1029.
  • 7Lazar D., M. Bottino, M. Ozcan, L. Valandro, R. Amaral, V. Ussui, A. Bressiani. Y-TZP ceramic processing from coprecipitated powders: A comparative study with three commercial dental ceramics [J].Dental Materials,2008,24(12): 1676-1685.
  • 8Gonudez P. New biomorphic SiC ceramics coated with bioactive glass for biomedical applications [J].Biomaterials,2003,24 (26):4827- 4832.
  • 9Sadat-Shojai Mehdi, Mohammad Atai, Azizollah Nodehi, Leila Nasiri Khanlar. Hydroxyapatite nanorods as novel fillers for improving the properties of dental adhesives: Synthesis and application [J].Dental Materials,2010,26(5):471-482.
  • 10Yoshitake K, T Takahsshi, M Hayashi, T Watanabe, J Zhao, Y Abiko. Fibrenectin and Focal Adhesion Kinsse Gene Expression in Dog Mandible Implanted by β-TCP [J]joumal of Oral Tissue Engineering,2010,8(1):1-8.

引证文献1

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部