摘要
以低碳钢或铸铁为阳极,以不锈钢、碳钢为阴极,槽压1.5—3.5V、电流密度0.1—0.2A、温度10—20℃电解合成高铁酸钾,为其工业化生产提供了重要参数。
The method by taking low-carbon steel or cast iron as possitive pole, stainless steel or carbon steel as negtive pole is used under 1. 5 to 3. 5 volt. 0. 1 to 0. 2A and 10 ℃ to 20 ℃ to make K2FeO4 through electrolysis, and it also provides significant data for mass production.
出处
《山西师大学报(自然科学版)》
1998年第1期46-48,共3页
Journal of Shanxi Teachers University(Natural Science Edition)