摘要
本文采用化学合成手段制备了不同粒径和Ey3+掺杂浓度的纳米Y2O3:Eu3+粉体,并采用包膜的方法对纳米粉体进行表面处理.通过对荧光性能的研究,发现纳米Y2O3:Eu3+粉体的激活剂临界浓度明显提高,并导致材料的荧光强度明显增强.另外,经包膜处理的纳米Y2O3:Eu3+粉体,由于有效地消除了表面悬空键。
Nano-scale Y2O3:Eu3+ powders with different grain sizes and Eu3+ concentrations were prepared by chemical process, and dealed with coating. It was found that the Eu3+ critical concentration of nano-scale Y2O3:Eu3+ powders was increased obviously, and it caused the luminescentintensity improved. In addition, because the hanging bonds on the surface of coating nano-scaleY2O3:Eu3+ powders were mostly vanished, the luminescent intensity was further enhanced.