不同窝洞处理剂对银汞合金充填微渗漏的影响 被引量:13

Effect of various materials or techniques on the microleakage at the material/cavity wall interface of amalgam restoration
暂未订购
导出
摘要 目的:探讨减少银汞合金充填后边缘微渗漏的有效方法。方法:选择无龋的离体磨牙48个,随机分为4组,每个牙分别制面洞、颊面颈1/3洞。比较几种窝洞洞壁处理后对微渗漏的影响。结果:银汞合金充填1个月后,10%EDTA处理窝洞组、10%EDTA加护洞漆组与空白组之间的边缘微渗漏无明显差异,而含3%FeCl3的10%枸橼酸(10-3液)处理加银汞合金粘结剂组则明显减少微渗漏。 Aim:To find effective methods to decrease microleakage at the material/cavity wall interface of amalgam restoration. Methods:Selected 48 non-carious extracted molars, and divided them into 4 groups, then made occlusal or cervical cavities and filling with amalgam in each tooth,comparing the extent of microleakage among groups. Results:One month after amalgam restorations, there were no significant difference among the micrdeakage of 10%EDTA group, 10%EDTA+cavity varnish and control group. Howerer,10%Citric acid containing 3%FeCl 3 with amalgam bonding agent significantly reduced the microleakage. Conclusions: It indicated bonding amalgam restorations reduced the microleakage significantly.
出处 《牙体牙髓牙周病学杂志》 CAS 1998年第3期185-186,共2页 Chinese Journal of Conservative Dentistry
关键词 银汞合金 微渗漏 粘结剂 护洞漆 牙科材料学 amalgam microleakage bonding agent cavity varnish
  • 相关文献

参考文献2

共引文献13

同被引文献42

引证文献13

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部