期刊文献+

TiO_2光催化降解孔雀石绿活性的影响因素 被引量:5

The study of photocatalysis degradation of malachite-green over TiO_2
在线阅读 下载PDF
导出
摘要 对持久性难降解的有机染料孔雀石绿溶液的光催化降解过程进行研究,考察了孔雀石绿的初始浓度、催化剂的用量、溶液的初始pH值以及H2O2的加入量等条件变化对孔雀石绿的脱色率的影响.实验结果表明,光照时间和其他实验条件均相同时,孔雀石绿溶液的初始浓度为2 mg.L-1和5 mg.L-1时其脱色率较高;最佳的催化剂用量为1 g.L-1;溶液初始pH值为8的弱碱条件下降解效果较好;氧化剂H2O2的加入量为0.1 Vt.%时光催化反应效果较佳. The influences of various parameters such as the initial concentration of Malachite Green,the amount of catalyst,initial pH and the amount of H2O2 had been investigated.With the same irradiation time and other experimental conditions,the decolorization rate of degradation of malachite-green was higher when the initial concentration was 2 mg·L-1 and 5 mg·L-1.It also showed that the optimum dosage of catalyst and H2O2 was 1g·L-1 and 0.1 Vt.% respectively.In addition,when pH=8 the degradation effect of malachite-green was better.
出处 《闽江学院学报》 2009年第5期98-102,共5页 Journal of Minjiang University
基金 闽江学院科研育苗项目(YKY06002)
关键词 TIO2 光催化 孔雀石绿 降解 脱色率 TiO2 photocatalysis malachite-green degradation decolorization rate
  • 相关文献

参考文献9

二级参考文献142

共引文献158

同被引文献56

引证文献5

二级引证文献13

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部