摘要 目的:研究氮化钛涂层对循环摘戴后圆锥型套筒冠固位力的影响。方法:使用精密数控车床制作标准金属内、外冠试件14对,随机分成2组(实验组和对照组),每组7对,在实验组套筒冠内冠表面和外冠内面沉积2μm氮化钛(TiN),未镀TiN组为对照组,测定2组套筒冠经循环摘戴后固位力值。采用SPSS13.0软件包对实验数据进行成组t检验统计分析。结果:镀TiN组套筒冠初始固位力较未镀膜组小,2组固位力随循环次数的增加而降低,未镀膜组固位力下降速度较镀膜组更为显著。镀TiN组套筒冠在循环3000次后固位力开始下降,3000次前和7000次后固位力下降平缓。结论:圆锥型套筒冠内、外冠沉积氮化钛涂层可以降低套筒冠固位力衰减速度,能够保持持久的固位力。 Objective:To evaluate the effect of TiN coating on retentive force of eonus telescopic crowns after repeated insertion/ separation tests. Methods : Fourteen pairs of standard metal specimens fabricated by precision Computer Numerical Control ( CNC ) Lathe were randomly divided into experimental group and control group, seven pairs in each group. The external surfaces of inner crowns and internal surfaces of outer crowns of experimental group were coated with a 2.0 μm titanium uitride (TiN) by multi-are ion plating method. The group without titanium nitride coating was served as control. The retentive forces of two group telescopic crowns was investigated by repeated insertion/separation tests. Statistical analysis of group t-test was performed by SPSS 13.0 software package. Results : The results demonstrated that the initial retentive force of titanium nitride group in our study were lower than that of un- coated titanium nitride group. The retentive forces of two groups gradually decreased depending on the number of insertion/separation cycles and the rate of retention attenuation was found to be statistically significant. It was also shown that the retentive force of titani- um nitride coating group began to decrease after 3 000 cycles and declined slowly not only before 3 000 cycles but also after 7 000 cycles. Conclusion : Titanium nitride coating deposited on external surface of inner crowns and internal surface of outer crowns can sig- nificantly decrease retention attenuation rate of conus telescopic crowns and maintain persistent retentive force.
出处 《实用口腔医学杂志》 CAS CSCD 北大核心 2009年第4期479-481,共3页 Journal of Practical Stomatology
关键词 氮化钛 套筒冠 固位力 循环摘戴 Titanium nitride Telescopic crowns Retention Repeated insertion/separation
  • 相关文献

参考文献6

  • 1解保生,朱惠兰,李爱霞,徐芸.口腔正畸用磁块镀氮化钛膜后抗人工唾液腐蚀研究[J].实用口腔医学杂志,2003,19(3):257-259. 被引量:18
  • 2解保生,李爱霞,朱惠兰,徐芸.口腔正畸用磁块镀氮化钛膜后抗腐蚀性能的定量研究[J].实用口腔医学杂志,2005,21(1):50-53. 被引量:9
  • 3Pappas MJ,Makris G,Buechel FF.Titanium nitride ceramic film against polyethylene.A 48 million cycle wear test[J].Clin Orthop Relat Res,1995,(317):64-70.
  • 4Tek Z,Güg(o)r MA,Cal E,et al.A study of the mechanical properties of TiN coating of Cr-Ni alloy[J].Surface and Coatings Technology,2005,196(1-3):317-320.
  • 5Hai K,Sawase T,Matsumura H,et al.Corrosion resistance of a magnetic stainless steel ion-plated with titanium nitride[J].J Oral Rehabil,2000,27(4):361-366.
  • 6Minagi S,Natsuaki N,Nishigawa G,et al.New telescopic crown design for removable partial dentures[J].J Prosthet Dent,1999,81(6):684-688.

二级参考文献5

  • 1国家技术监督局.GB/T 16545-1996.金属和合金的腐蚀.腐蚀试样上腐蚀产物的清除[M].北京:中国标准出版社,1997..
  • 2Kedici SP, Aksut AA, Kilicarslan MA, et al. Corrosion behavior of dental metals and alloys in different media. J Oral Rehabil, 1998, 25(10):800.
  • 3The International Organization For Standardization( ISO ). 10271. 2001. Dental metallic materials-Corrosion test methods. Switzerland. 2002-11.
  • 4陈文,王光华,黎完模.pH对银汞合金腐蚀性能的影响[J].中华口腔医学杂志,1997,32(5):297-299. 被引量:3
  • 5解保生,朱惠兰,李爱霞,徐芸.口腔正畸用磁块镀氮化钛膜后抗人工唾液腐蚀研究[J].实用口腔医学杂志,2003,19(3):257-259. 被引量:18

共引文献22

同被引文献56

引证文献2

二级引证文献3

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部