介结了云南天文台太阳光谱仪1988年进行的重镀11块照相透镜增透膜以及镀膜后的使用情况。重镀增透膜前照相透镜的透过率已降低到77%~84%,重镀后提高到92%~98%。相对于镀膜之前的透过率数值提高14%~26%,照相露光时间缩短1倍左右。
In order to prepare the solar observation during the solar maximum of the 22nd cycle, the reflection reducing flim was recoated for the eleven photographic lenses of the solar spectrograph at Yunnan Observatory in 1988. The status of exploitation is given for the spectrograph after the recoating. The transmissivity of these lenses is only 77%-84% before and 92%-98% after recoating,i.e. the transmissivity of the lenese is increased 14%-26%. The exposure time of the photograph of the spectrograph is only half of that before the recoating. Thses lenses have been used for about 8 years since they were recoated.