摘要
1INTRODUCTIONPowderinjectionmoulding(PIM)isanewprocessformanufacturingnearnetshapepartswithadvantagesoflowcost,highperformanc...
To control the defects in thermal debinding stage, low temperature thermal debinding behavior of wax in the multi component binder for tungsten heavy alloy was studied. The wax burnout temperature is below 250 ℃, at which the defects mainly occur. The debinding rate is controlled by the diffusion of wax in the polymer to the inner surface of pores and then to the external environment. The experiment proved the amount of removed wax as an exponential function of time, the reciprocal sample thickness and temperature coeffcient.
出处
《中国有色金属学会会刊:英文版》
EI
CSCD
1999年第1期95-100,共6页
Transactions of Nonferrous Metals Society of China