摘要 综述了用EAF-LF-VD-WF-CC工艺流程生产低氮钢的现状及采取的主要技术措施。降氮措施有:电炉内激烈的碳沸腾、造泡沫渣、EBT出钢及采用DRI,VD炉内真空底吹氩搅拌;保护措施有:LF炉内气氛控制及连铸钢包与中间罐间的长水口加氩气环保护。 The status of main technological measures adopted for producing low nitrogen steel by EAFLF-VD-WF-CC process has been reviewed in this paper. To produce low nitrogen steel, the measures includevigorous CO boiling, slag foaming, EBT plocess, charging DRI in EAF, and vacuum argon bottom stirring inVD unit, and to protect nitrogen pick up, the methods include atmosphere controlling in LF and shrouding bylong ceramic nozzle and Ar ring between ladle and tundish during concasting are also presented.
机构地区 北京科技大学
出处 《特殊钢》 北大核心 1998年第1期1-6,共6页 Special Steel
关键词 炼钢 降氮 脱氮 电炉炼钢 Steelmaking,Nitrogen Removal,EAF-LF-VD-WF-CC Process
  • 相关文献

参考文献2

  • 1曹广畴.现代板坯连铸[M]冶金工业出版社,1994.
  • 2S. Ban-Ya,F. Ishii,Y. Iguchi,T. Nagasaka. Rate of nitrogen desorption from liquid iron-carbon and iron-chromium alloys with argon[J] 1988,Metallurgical Transactions B(1):233~242

同被引文献175

引证文献25

二级引证文献96

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部