期刊文献+

热处理对MDF力学性质的影响 被引量:1

Influence of Heat Treatment on Mechanical Properties of Medium Density Fiberboard
在线阅读 下载PDF
导出
摘要 对市场随机购买的中密度纤维板(MDF)进行热处理,以期改善其力学性质。采用全因素试验方法,对影响MDF热处理效果的因子进行了分析。结果表明:热处理温度、时间,以及不同的生产厂家和产品厚度,对板材的主要力学性质指标可产生一定的影响。建议:当产品中的胶黏剂未完全固化时,可以采用热处理工艺以提高其内结合强度。 Small samples of medium density fiberboard were treated at various temperatures and durations in a dry oven. The mechanical properties of these samples were evaluated to examine the effect of the heat-treatment. The results showed that temperature has a significant effect on the modulus of rupture while duration exhibited considerable impact on internal bond and modulus of elasticity. It was observed that heat treatment could improve internal bond when the press time was not long enough to cure the binder.
出处 《木材工业》 北大核心 2008年第6期14-16,共3页 China Wood Industry
基金 国家重点基础研究发展计划(973计划)项目(2007CB210201) 国家自然科学基金(30671634) 中南林业科技大学青年科学研究资助项目(05036B)
关键词 中密度纤维板(MDF) 力学性质 热处理 medium density fiberboard mechanical properties heat treatment
  • 相关文献

参考文献8

二级参考文献83

  • 1中国林学会木材工业分会 湖南人造板厂.中密度纤维板工业发展问题研讨会论文集[M].长沙,1996,10..
  • 2王天佑.中密度纤维板专辑[M].中国林业科学研究院木材工业研究所,1985,1..
  • 3张勤丽,张齐生,张斌渊,译.木材应用基础[M].上海:上海科学技术出版社,1986.
  • 4Sailer M, Rapp A O, Leithoff H, et al. 2000. Vergutung yon Holz dutch Anwendung einer 01- Hitzeehandlung. Holz als Roh-und Werkstoff, 58:15 - 22
  • 5Sanderman W, Augustin H. 1963a. Chemical investigations on the thermal decomposition of wood. Part Ⅱ: Investigations by means of the differential thermal analysis. Holz als Roh-und Werkstoff, 21 : 305 - 315
  • 6Sanderman W, Augustin H. 1963b. Chemical investigations on the thermal decomposition of wood. Part I: Stand of research. Holz als Roh-und Wetkstoff, 21: 256 - 265
  • 7Schneider A, Rusche H. 1973. Sorption-behaviour of Beech and Spurcewood after heat treatments in air and absence of air. Holz als Roh-und Werkstoff, 31 : 313 - 319
  • 8Schneider A. 1971. Investigations on the influence of heat treatments within a range of temperature from 100℃ to 200℃ on the modulus of elasticity, maximum crushing strength, and impact work of Pine sapwood and Beechwood. Holzforschung, 29:431 -440
  • 9Schneider A. 1973. Investigation on the convection drying of lumber at extremely high temperatures. Part Ⅱ: Drying degrade, changes in sorptlon, colour and strength of pine sapwood and beech wood at drying temperatures from 110℃ to 180℃. Holz als Roh-und Werkstoff, 31: 198- 206
  • 10Schwanninger M, Hinterstoisser N, Gierlinger N, et al. 2004. Application of fourier transform near infrared spectroscopy (FT-NIR) to thermally modified wood. Holzforschung, 62:483 - 485