摘要 芳纶纤维无石棉离合器面片综合机械性能好,加工性能优越,工艺相容性好,无污染,产品使用寿命长,且比重轻,爆裂强度高,摩擦性能稳定,高温300℃衰退小,磨损小。本次研制的面片主要性能达到德国雷贝斯托同类产品的技术水平。 The non-asbestos clutch facing with Kcvlar has good comprehensive mechanical properties, excellent processing performances and fine technical compatibility with other materials. Thc product has long service life , light specific gravity, high bursting strength and is nonpolluting. The friction performance of this product is stable, which has less recession and is wear-resistant under 300%. The main pertbrmanccs ofthis developed product roach the same technologic level compared with the Raybestos like products made in Germany
作者 蔡仁华
出处 《非金属矿》 CAS CSCD 北大核心 2008年第5期47-49,68,共4页 Non-Metallic Mines
关键词 离合器面片 芳伦纤维 产品研制 clutch facing Kevtar product developing
  • 相关文献

参考文献5

二级参考文献13

  • 1顾澄中,胡福增,吴叙勤.摩阻材料中基体树脂的共混改性研究[J].非金属矿,1995,18(2):58-60. 被引量:9
  • 2(德国)迪弗泽林.在热负荷作用下工业制动器摩擦面上摩擦系数级温度变化[J].起重运输机械,1983,10:12-16.
  • 3任增茂 等.增强型非石棉缠绕式离合器面片的研究开发[A]..国际摩擦与密封材料技术交流会论文集[C].北京:摩擦密封材料协会,2002.104~105.
  • 4任增茂 等.非石棉缠绕式离合器面片成型工艺对产品性能的影响[J].摩擦密封材料,2002,(4).
  • 5瞿雄伟,王晓平.汽车制动用无石棉摩擦材料[J].中国塑料,1997,11(2):16-23. 被引量:8
  • 6Jacko M G, Tsang P H S, Rhee S K. Automotive friction materials evolution during the past decade[J].Wear,1984,100:503-515.
  • 7Kim S J, Jang H. Friction and wear of friction materials containing two different phenolic resins reinforced with aramid pulp[J].Tribology International,2000, 33:477-484.
  • 8Verma A P, Vishwanath B, Rao C V S K. Effect of resin modification on friction and wear of glass phenolic composites[J].Wear, 1996,193 (2):193-198.
  • 9周继承,黄伯云.列车制动摩擦材料研究进展[J].材料科学与工程,1999,17(2):91-93. 被引量:34
  • 10刘晓辉,赵颖,王致禄.摩擦材料用酚醛树脂胶粘剂的研究现状[J].粘接,1999,20(S1):27-32. 被引量:13

共引文献56

同被引文献10

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部