期刊文献+

物理细化工艺对黄麻纤维性能的影响 被引量:9

Effect of physical modification on properties of jute fibers
在线阅读 下载PDF
导出
摘要 介绍黄麻化学物理联合精细化工艺过程,为提高黄麻纤维的可纺性,研究不同物理细化路线、工艺参数及细化步骤对黄麻纤维力学性能的影响规律,通过对比分析黄麻纤维的线密度、长度和力学性能指标得出:梳理工艺对黄麻纤维线密度、长度和强力都有非常大的影响,是黄麻物理精细化过程中控制的关键因素;经过预处理—长麻牵切—梳理工艺得到的黄麻纤维线密度为16.65 dtex,长度为30.16 mm,可用于棉纺工艺流程。 Physicochemieal refining process for jute fibers was presented. With the aim to improve the spinnability of the jute fiber, the effects on mechanical properties of jute fibers in varying processes, parameters, and refining steps were analyzed and discussed. By analyzing the average length, linear density, and breaking strength of jute fibers obtained by different processes, the results show that hackling process has great effect on the average length, linear density, and breaking strength of jute fibers and is a key controlling factor in the physical refining; jute fibers with the fineness of 16.65 rex and length of 30.16 mm that are obtained through pretreatment-long fiber drawing/cutting-hackling are suitable for cotton spinning system.
出处 《纺织学报》 CAS CSCD 北大核心 2008年第7期27-29,共3页 Journal of Textile Research
关键词 黄麻 物理细化 牵切 梳理 jute physical refining draw-cutting hackling
  • 相关文献

参考文献10

二级参考文献19

  • 1张小英.黄麻纤维的应用和发展[J].国外丝绸,2004,19(6):38-39. 被引量:8
  • 2杜兆芳,曹建飞,方木胜.黄麻酶脱胶工艺研究[J].安徽农业大学学报,2005,32(1):98-100. 被引量:9
  • 3李升平.我国汽车用纺织品开发前景[J].中国纺织管理,1996(8):34-38. 被引量:1
  • 4徐谷仓.染整织物短流程前处理[M].北京:中国纺织出版社,1999..
  • 5钱章武 杨松年.黄麻与洋麻的脱胶和分级检验[M].北京:纺织工业出版社,1988.16-37,117-120.
  • 6浙江麻纺织厂黄麻纺纱手册编写组.黄麻纺纱手册[M].北京:纺织工业出版社,1988.11-37.
  • 7姜繁昌 邵宽 周家谔.黄麻纺纱学[M].北京:纺织工业出版社,1985.10-13.
  • 8杨淑惠.植物纤维化学[M].北京:中国轻工业出版社,2001.26-64.
  • 9江苏紫金花纺织科技股份有限公司.黄麻纤维精细化及纺织加工技术和产品[Z].2005.
  • 10T N Chakraborty,A Sarkar.Jute Processing with/without Softener Machine[J].The Indian Textile Journal,1998,99(1):90-96.

共引文献43

同被引文献94

引证文献9

二级引证文献56

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部