唐钢热轧热镀锌生产线调试初期的产品在加工使用过程中,出现了脱锌的现象。利用电镜、辉光光谱仪等分析手段对此进行了试验研究,分析缺陷产生原因,并寻找解决方案。
Zinc scaling was occurred in the early products of hot rolled galvanization line in TanShan Iron and Steel Limited Cooperation. In order to find the generating cause and treating method, electron microscope and luminance optical spectrometer have been used in investigation.
出处
《上海金属》
CAS
2007年第5期189-192,共4页
Shanghai Metals
关键词
热轧镀锌板
锌层脱落
电子显微镜
辉光光谱仪
Hot Rolled Galvanization Plate, Zinc Scaling, Electron Microscope, Luminance Optical Spectrometer