摘要
作者利用机械合金化制备了WxCu(100-x)(x=0~100)合金.当x>80时,获得的W-Cu合金是一种完全的W(Cu)固溶体.实验结果表明,球磨70h后。
By MA have been synthesized W x Cu (100- x ) ( x =0 ̄100) alloys. When x >80, the alloy is a total solid solution. The results show that the grain size of the solid solution by milling 70 h is about 10 nm.
出处
《华北工学院学报》
1996年第4期289-293,共5页
Journal of North China Institute of Technology