摘要
列举了强力旋压常见缺陷,例如裂纹、起皮、堆积、粘结、鼓包、内壁划伤、扩径等,分析了产生的原因,针对坯料和旋压工艺参数,简要探讨了应对措施。
The familiar defects of powerful spinning have been listed, such as crack,rising skin, gluing knot, piling, speed bulge, the wound inside the wall, expanding etc, with analysis of the cause and probing into treatments according to the basic fondant and spinning craft parameters.