期刊文献+

基于J参量的管道环焊缝表面缺陷塑性撕裂评定 被引量:2

Ductile tearing assessment of surface flaw in circumferential weld of pipe-line based on J integral parameter
在线阅读 下载PDF
导出
摘要 基于英国标准BS7910中的三级评定规程(3C),采用SC.ENG(表面裂纹工程估算方法)J积分工程估算方法对承受纯弯曲载荷作用的管道环焊缝表面裂纹进行塑性撕裂评定。以X56钢管道环焊缝内表面缺陷为算例,讨论了选用J参量进行含缺陷结构的塑性撕裂评定时,裂纹尺寸和断裂评定参量选取对评定曲线及评定结果的影响规律,提出了在J积分评定中选择参量Jmat确定评定点较Jg更趋合理。研究内容不仅对管线铺设安全评价具有指导作用,而且对含缺陷结构的塑性撕裂评定在工程上的应用具有推广和借鉴价值。 Based on level three programme(ductile tearing assessment) of assessment standard BS7910,ductile tearing assessment of surface flaw in circumferential weld of pipe-line under pure bending load was proceeded by using J integral engineering estimate method of SC.ENG.By taking X56 steel pipeline as an example,effects on assessment curve and evaluating results were given by flaw dimension and fracture parameter choosing were discussed,and the assessment point was put forward that Jmat is more reasonable than Jg in determining assessment points while choosing J integral parameter to make a ductile tearing assessment of flaw in metal structure.The research results are not only taken as a guide on safty evaluation in pipeline construction,but also can make engineering application of the ductile tearing assessment of structure with flaw more popular and referentia.
出处 《焊接学报》 EI CAS CSCD 北大核心 2007年第2期59-62,66,共5页 Transactions of The China Welding Institution
关键词 英国标准BS7910 J积分 环焊缝 表面缺陷 塑性撕裂评定 BS7910 J integral circumferential weld surface flaw ductile tearing assessment
  • 相关文献

参考文献3

  • 1British Standard Institution.BS7910-1999:(Incorporating amendment No.1) Guide on methods for assessing the acceptability of flaws in metallic structure[S].
  • 2BS7448.确定金属材料断裂阻力曲线和裂纹稳定扩展启裂值的方法[S]Part Ⅳ.,1997..
  • 3刘月丽,霍立兴,张玉凤.LBB.ENG3 J积分估算方法对国产管道的适用情况[C]∥第九次全国焊接学术会议论文集(Ⅱ),1999:189-192.

同被引文献23

  • 1类维生,陈丙森.分形用于金属断裂研究的力学量选择问题[J].金属学报,1994,30(6). 被引量:5
  • 2琚正挺,宣天鹏.分形计算方法及在材料表界面中的应用[J].稀有金属快报,2006,25(3):1-5. 被引量:6
  • 3杨小彬,庄茁,居来提.买买提肉孜.天然气管道动态断裂参数与裂纹速度关系的研究[J].工程力学,2006,23(A01):145-150. 被引量:5
  • 4全国钢标准化技术委员会.GB/T228-2002金属材料室温拉伸试验方法[S].北京:中国标准出版社,2002:1-15.
  • 5仇仲翼.应力强度因子手册[M].北京:科学出版社,1993.
  • 6全国钢标准化技术委员会.GB2038-91金属材料延性断裂韧度JIC试验方法[S].北京:中国标准出版社,国家技术监督局,1991:1-21.
  • 7Nageswara R B, Acharya A R. Failure assessment on M300 grade maraging steel cylindrical pressure vessels with an internal surface erack[J]. International Journal of Pressure Vessels and Piping, 1998, 75(7): 537- 543.
  • 8Tada H, Paris P C, Irwin G R. The stress analysis of cracks handbook[M]. Pennsylvania: Del Research Corp, 1973: 195- 210.
  • 9Griffith A A. The phenomena of rupture and flow in solids[M]. London: The Royal Society, 1921: 197-198.
  • 10Barenblatt G I. The mathematical theory of equilibrium cracks formed in brittle fracture[M]. Virginia: National Technical Information Service, 1962: 100-102.

引证文献2