摘要
借助DC-150多冲试验机,探讨了非组织因素时20CrMnMo钢表面剥落的影响。结果表明,端面起始剥落寿命主要取决于冲击能量和冲击频率,也和端面粗糙度有关。
he influence of non-microstructure factors on peeling off of 20CrMnMo steel was investigated by using DC-150 machine.the results showed that the life of initial peeling off depending on impact energy and impact frequency,and it is also related to surface roughness.
出处
《材料科学与工艺》
CAS
CSCD
北大核心
1996年第1期29-33,共5页
Materials Science and Technology
关键词
端面粗糙度
起始剥落寿命
凿岩机活塞
repeated impact test,impact energy,impact frequency,surface roughness,life of ini tial peeling off