摘要
将含锗石英玻璃废料在料碱质量比1∶4及820℃的条件下焙烧2.5 h,再经特殊工艺处理,然后进行酸化及蒸馏,锗的回收率由90%提高到93%以上.
By alkaline roasting 2.5 h at 820℃ and specially treatment ,acidify with sulphate acid and distillation et al. germanium is extracted from a quartz residue containing germanium. Results show that the recovery of Germanium can be rised from 90% to 93%.
出处
《广东有色金属学报》
2006年第1期6-7,共2页
Journal of Guangdong Non-Ferrous Metals
关键词
含锗石英玻璃废料
工艺
提取锗
quartz residue containing germanium
technoloyg
germanium recovery