摘要
叙述了近年来针对高铁锌精矿冶炼工艺所开展的研究工作,详细介绍了高铁锌精矿中铁的自催化—高温加压浸出工艺。工业试验表明,该工艺锌浸出率达98.05%,铁浸出率为29.22%,可有效地实现锌的选择性浸出。
This paper describes the research work about smehing process of high-iron zinc sulfide concentrate in recent years and presents in details the self-catalyzing-high-temperature pressure leaching of iron in the high-iron zinc sulfide concentrate.The commercial test shows that this and an iron leaching rate of 29.22%, thus realizing selective process can achieve a zinc leaching rate of 98.05% leach of the zinc effectively.