摘要
研究了防止超细高氯酸铵(UFAP)在贮存过程中聚结的表面改性方法以及改性后的超细高氯酸铵对高燃速推进剂性能的影响。
Inorder to keep UFAP from coagulation during storage,various surfacemodifications of UFAP were studied.The influence of using modified UFAP upon thecharacteristics of the high burning rate propellant is described.
出处
《含能材料》
EI
CAS
CSCD
1995年第2期26-30,共5页
Chinese Journal of Energetic Materials