摘要
在酸(H2SO4、HNO3-H2SO4)及碱(NaOH、NH4OH、Ca(OH)2)性介质中分别对合砷的难选难冶金矿(4.9g/tAu)进行了加压氧化预处理研究,表明金的氰化浸出率可由15%提高到85%。
In this paper the pretreatments of arsenical refractory gold ore with pressure oxidation process in an acid aqueous solution (H2SO4, HNO3-HNO3) and alkaline aqueous solution (NaOH, Ca (OH)2, NH4OH)have been shidied respectively. The experimental results show that the eganide leaching rate can be improved from 15%to over 85%by pretreatment of pressure oxidation.
出处
《黄金》
CAS
北大核心
1995年第3期23-26,共4页
Gold
关键词
含砷难冶金矿
加压氧化酸浸
金
熔炼
浸出
arsenical refractory gold ore
pressure oxidation follwed by aeid leach
pressure oxidation followed by alkalige leaching.