摘要
本研究以SiC作还原剂,采用氧化焰烧成,试制成功了在1250~1260℃下烧成的铜红釉,克服了传统的还原焙烧成方法的不足,简化了生产工艺,提高了铜红釉的成品率。
Overcoming the shortage of traditional firing method by reducing flame, copper-red glaze fired in oxidizing atmosphere using SiC as reducing agent at 1250-1260℃ is present-ed with advantages of simple production procedure and high end-product rate.